MOX-Tape ™®
UNSUPPORTED, SELF-ADHERING, TRIANGULAR, SILICONE TAPE
PHYSICAL AND ELECTRICAL PROPERTIES
Mox-Tape 600-T Triangular Series Tape is produced in the form of a triangular cross section with a colored guide line running along the peak of the triangle. The guide line facilitates winding of the tape so minimum overlapping is obtained while maximum physical and electrical properties are retained. The tape is interleaved with a quick release film. It is self-bonding and self-fusing. After curing at room temperature for 24 hours, the tape forms an inseparable silicone layer that must be cut for removal.
MOX-Tape® 600-T Series Unsupported Triangular Guideline Tape | |||||
Arlon Product No. | Reference MOX-Tape® | Width (inches) | Thickness (inches) | Color | Description: |
T2020-B004 | 602 | 1.00″ | 0.020″ | Black | Silicone, self-fusing tape. Meets Commercial Item Description A-A-59163 (supersedes US Military Specification MIL-I-46852C) except for packaging. |
T2020-R004 | 602 | 1.00″ | 0.020″ | Red | |
T2030-R004-12 | 603 | 1.00″ | 0.030″ | Red | 12.0 yards long, silicone, self-fusing tape. |
T2040-B004 | 604 | 1.00″ | 0.040″ | Black | |
T2040-R004 | 604 | 1.00″ | 0.040″ | Red | Meets Commercial Item Description A-A-59163 (supersedes US Military Specification MIL-I-46852C) except for packaging. |
T2060-B006 | 606 | 1.50″ | 0.060″ | Black |
Archived info: Download PDF
Dielectric Strength (Before Stretching) |
||
602-1 | 450 VPM Minimum | |
603-1 | 350 VPM Minimum | |
604-1, 604-1 1/2 | 300 VPM Minimum | |
605-1, 605-1 1/2 | 275 VPM Minimum | |
606-1 1/2 | 250 VPM Minimum | |
607-1 1/2 | 225 VPM Minimum | |
Hardness | Shore “A” (ASTM D2240) | 50 +/- 10 |
Tensile Strength | (ASTM D412) | 700 psi minimum |
Elongation | At Break (ASTM D412) | 350% Minimum |
Temperature Range | -65º to +500º F | |
Resistivity | Volume Resistivity (ASTM D991) | 1013 ohm/cm. Minimum |
Adhesion | Tackiness (ASTM D2148) | 2 P.P.I. |
Military Specification | A-A-59163 Cl I, Ty II, DMS 2186 Ty II, GE 3003M70PO1, MIL-I-46852C Type II, RMS 315 Ty II |
NOTE: The above properties are published as a guide only, and should not be used for specification without testing in your own laboratory.